The improvement of oxidation resistance, mechanical and tribological properties of W2N films by doping silicon

Show simple item record

dc.contributor.author Ju, H.
dc.contributor.author He, S.
dc.contributor.author Yu, L.
dc.contributor.author Asempah, I.
dc.contributor.author Xu, J.
dc.date.accessioned 2023-01-19T14:32:07Z
dc.date.available 2023-01-19T14:32:07Z
dc.date.issued 2017
dc.identifier.other 10.1016/j.surfcoat.2017.03.058
dc.identifier.uri https://www.sciencedirect.com/science/article/abs/pii/S0257897217303171
dc.identifier.uri http://atuspace.atu.edu.gh:8080/handle/123456789/2512
dc.description.abstract W-Si-N composite films were deposited on both stainless steel and silicon wafers using a reactive magnetron system. The silicon content of the film was varied to evaluate the effect of silicon on films' elemental composition, microstructure, oxidation resistance, mechanical and tribological properties. These series of test were conducted using X-ray diffraction (XRD), X-ray photoelectron spectroscopy (XPS) and high resolution transmission electron microscopy (HRTEM) analytical tools. The W-Si-N films showed a two-phase structure of solid solution face-centered cubic (fcc) W(Si)Nx and an amorphous Si3N4. The thermal stability and the oxidation resistant temperature of W-Si-N films increased from about 380 °C at 0 at% Si to about 650 °C at 31.2 at% Si with the incorporation of Si into W2N matrix. The hardness of the films increased continuously from 26 GPa at 0 at% Si to 40 GPa at 23.5 at% Si which was due to solid strengthening and fine-grained strengthening. The silicon content affected the tribological properties of the film at room temperature but this was mainly influenced by the yield pressure, H/E ratio and elastic recovery, since lubricant tribo-film WO3 was detected on all surfaces of the W-Si-N films. There was an initial gradual decrease in average coefficient of friction and wear rate until a minimum, but a further increase in silicon content resulted in increase in both friction coefficient and wear rates. The least coefficient of friction and wear rate values were 0.30 and 8.7 × 10− 8 mm3/N·mm at 23.5 at% Si. en_US
dc.language.iso en_US en_US
dc.publisher Surface and Coatings Technology en_US
dc.relation.ispartofseries vol;317
dc.title The improvement of oxidation resistance, mechanical and tribological properties of W2N films by doping silicon en_US
dc.type Article en_US


Files in this item

Files Size Format View

There are no files associated with this item.

This item appears in the following Collection(s)

Show simple item record

Search ATU Infohub


Browse

My Account